Blocks of Flats, 2007
Project
- Corroding steel lintels over windows and moisture ingress into cavity
- Cracking due to thermally induced movement
Solution
- Bersche-Rolt stainless steel reinforcement was installed to support the brickwork prior to the
installation of new galvanised steel angles and cavity trays
- Cracks were raked out and repaired with Bersche-Rolt bonding mortar
|